Free CWI Practice Test: AWS CWI Part A Questions & Answers

CWI-Exams.com · CWI Part A Practice Test · Free online version with instant answers: https://cwi-exams.com/cwi-part-a-practice-test/
Last updated: November 2026 · AWS CWI Part A (Fundamentals)

Free CWI practice test for AWS CWI Part A: 30 exam-style questions with answers and explanations, plus a full interactive quiz.

Part A is the closed-book Fundamentals exam: 150 questions in 2 hours, and you need 72% to pass. These questions follow the same style, with close answer choices that test real understanding, not memorised wording.

150questions on real Part A
2 hrsexam time
72%pass mark
Closedbook
Get 2,500+ Part A questions →

About the AWS CWI Part A Exam

The AWS Certified Welding Inspector (CWI) exam has three parts, and you must score at least 72% on each. Part A, Fundamentals, is the broadest: it tests the technical knowledge every welding inspector needs, without a codebook.

PartFormatQuestionsPass mark
Part A: FundamentalsClosed book, computer-based15072%
Part B: PracticalHands-on, with AWS-provided equipment4672%
Part C: Code BookOpen book (e.g. AWS D1.1 or API 1104)50–6572%

Preparing for the codebook part too? Try our free API 1104 Part C practice exam.

What CWI Part A Covers

TopicWhat to know
Welding processesSMAW, GMAW, FCAW, GTAW, SAW and others: equipment, consumables, polarity, transfer modes, process limitations
Welding metallurgyHeat input, preheat, HAZ, hydrogen and hot cracking, carbon equivalent, stainless steel behaviour
Welding symbolsAWS A2.4 weld and NDE symbols: arrow/other side, sizes, lengths and pitch, supplementary symbols
Terms and definitionsAWS A3.0 welding terms, joint types, weld features
Destructive testingTensile, bend, Charpy, hardness, nick-break, fillet weld break and macroetch tests
Nondestructive examinationVT, PT, MT, UT and RT: principles, capabilities and limitations
DiscontinuitiesCracks, porosity, slag, incomplete fusion and penetration, undercut, overlap: causes and prevention
Procedures, qualification and documentsWPS, PQR, welder qualification, codes and specifications, inspector duties
CalculationsHeat input, unit conversions, tensile strength, fillet weld throat and similar inspection math
SafetyANSI Z49.1, fumes, radiation, electrical hazards, gas cylinder handling

Know the topics? Now test yourself under time.2,500+ Part A questions with explanations and mock exams.

Start practising →

Free CWI Practice Test: 30 Part A Questions with Answers

Answer each question as if it were the real exam, without notes. Pick an answer to see whether you’re right and why. Prefer paper? with an answer key.

Your score: 0 / 30

Part 1: Welding processes

Question 1
In the SMAW electrode classification E7018, the ’70’ indicates:
AWS A5.1 classificationE70XX electrodes deposit weld metal with a minimum tensile strength of 70 ksi. Yield strength is a separate, lower requirement.
Question 2
In the electrode classification E7018, the digit ‘1’ indicates the electrode is usable in:
AWS A5.1 classificationThe third digit gives the position: 1 = all positions, 2 = flat and horizontal fillet only, 4 = flat, horizontal, overhead and vertical-down.
Question 3
In GTAW, which current type puts most of the arc heat into the workpiece and gives the deepest penetration?
Process fundamentalsWith DCEN, roughly two-thirds of the heat goes into the work, giving deep, narrow penetration and keeping the tungsten cool. DCEP overheats the tungsten.
Question 4
Which GMAW metal transfer mode has the lowest heat input and is commonly used on thin sheet and open root passes?
Process fundamentalsIn short-circuiting transfer the wire touches the weld pool many times per second, giving the lowest heat input. Pulsed spray is lower than spray, but still higher than short-circuiting.
Question 5
Which welding process uses a blanket of granular flux so that the arc is not visible during welding?
Process fundamentalsIn SAW the arc is completely covered by a blanket of granular flux, so the arc is not visible during welding.
Question 6
Slag inclusions are NOT expected in welds made with which process?
DiscontinuitiesSlag comes from flux. GTAW uses an inert shielding gas and no flux, so slag inclusions are not expected (tungsten inclusions are its typical inclusion).

Part 2: Metallurgy and heat

Question 7
Hydrogen (cold) cracking requires which combination of factors?
Welding metallurgyHydrogen cracking needs hydrogen, a susceptible microstructure such as martensite, and tensile stress, at a temperature near ambient. Sulfur, phosphorus and bead shape are factors in solidification (hot) cracking.
Question 8
Solidification (hot) cracking in the weld metal is promoted by:
Welding metallurgyLow-melting impurities such as sulfur and phosphorus, combined with a deep, narrow bead shape and restraint, promote centerline solidification cracking.
Question 9
Calculate the heat input for 24 V, 200 A and a travel speed of 10 in./min.
CalculationsHeat input (J/in.) = (V × A × 60) / travel speed (in./min) = (24 × 200 × 60) / 10 = 28,800 J/in. = 28.8 kJ/in.
Question 10
The main reason for preheating a carbon steel with a high carbon equivalent is to:
Welding metallurgyPreheat slows cooling, so less martensite forms in the HAZ, and gives hydrogen time to escape. Both reduce the risk of hydrogen cracking.
Question 11
Austenitic stainless steels held for a time at about 800–1600 °F (425–870 °C) may suffer:
Welding metallurgyChromium carbides precipitate at grain boundaries in this range, depleting nearby chromium and making the steel susceptible to intergranular corrosion. Low-carbon (L) and stabilized grades reduce the risk.

Part 3: Welding symbols (AWS A2.4)

Question 12
A fillet weld symbol placed BELOW the reference line indicates the weld is to be made:
AWS A2.4Symbols below the reference line refer to the arrow side; symbols above it refer to the other side.
Question 13
On a fillet weld symbol, the dimension shown to the LEFT of the weld symbol is the:
AWS A2.4Fillet weld size goes to the left of the symbol. Length and pitch go to the right.
Question 14
A fillet weld symbol shows ‘2-6’ to the right of the weld symbol. This means intermittent welds:
AWS A2.4The first number is the length of each increment; the second is the pitch, measured center to center, not the gap between welds.
Question 15
A circle at the junction of the arrow and the reference line means:
AWS A2.4The circle is the weld-all-around symbol. A flag indicates a field weld.
Question 16
A groove weld symbol shows ‘1/2 (5/8)’ to the left of the symbol. This means:
AWS A2.4The depth of groove preparation (S) is shown first, and the groove weld size (E) follows in parentheses.
Question 17
Which finishing designation letter indicates grinding?
AWS A2.4Finishing letters: C = chipping, G = grinding, H = hammering, M = machining, R = rolling, U = unspecified.

Part 4: Testing and NDE

Question 18
Which NDE method can detect only discontinuities that are open to the surface?
Nondestructive examinationPT detects only surface-breaking discontinuities. MT finds surface and slightly subsurface discontinuities, but only in ferromagnetic materials.
Question 19
Magnetic particle testing cannot be used to inspect:
Nondestructive examinationMT requires a ferromagnetic material. Austenitic stainless steel is nonmagnetic.
Question 20
Which NDE method is generally best for detecting planar discontinuities such as lack of sidewall fusion and cracks in thick sections?
Nondestructive examinationUT is very sensitive to planar discontinuities. RT is best for volumetric discontinuities such as porosity and slag, and can miss planar flaws not aligned with the beam.
Question 21
A 0.505-in. diameter tensile specimen fails at a load of 14,000 lbf. The tensile strength is approximately:
CalculationsArea = π × (0.505/2)² = 0.200 in.². Tensile strength = 14,000 / 0.200 = 70,000 psi. Dividing by the diameter (27,700 psi) is the common mistake.
Question 22
The Charpy V-notch test is used to measure:
Destructive testingThe Charpy test measures the energy absorbed in breaking a notched specimen, usually at a specified low temperature.

Part 5: Discontinuities and visual inspection

Question 23
Undercut is most commonly caused by:
DiscontinuitiesToo much current or speed, a long arc or a poor angle melts away the base metal at the toe without filling it.
Question 24
Weld metal that flows onto the surface of the base metal without fusing to it is called:
DiscontinuitiesOverlap (cold lap) is weld metal protruding beyond the weld toe without fusion. Incomplete fusion is a lack of fusion inside the weld.
Question 25
For an equal-leg 45° fillet weld with 3/8-in. legs and a flat face, the theoretical throat is approximately:
CalculationsTheoretical throat = 0.707 × leg = 0.707 × 0.375 = 0.265 in.
Question 26
Lamellar tearing occurs in:
DiscontinuitiesLamellar tearing occurs in rolled plate with non-metallic inclusions when weld shrinkage stresses act through the plate thickness.

Part 6: Documents, qualification and safety

Question 27
Which document records the actual variables used to weld a procedure qualification test coupon and the test results?
Procedures and qualificationThe PQR records what was actually used and the test results. The WPS gives the ranges for production welding, supported by the PQR.
Question 28
Which AWS document is the specification for AWS certification of welding inspectors (CAWI, CWI and SCWI)?
Inspector certificationQC1 governs AWS certification of CAWIs, CWIs and SCWIs. B5.1 is the specification for the qualification of welding inspectors, which QC1 meets or exceeds.
Question 29
Safety in welding, cutting and allied processes is covered by which standard?
SafetyANSI Z49.1 covers safety in welding, cutting and allied processes. ANSI Z87.1 covers eye and face protection devices.
Question 30
In storage, oxygen cylinders must be separated from fuel-gas cylinders by a minimum of:
Safety (OSHA 1910.253)Oxygen cylinders in storage must be at least 20 ft (6.1 m) from fuel-gas cylinders or combustible materials, or separated by a noncombustible barrier at least 5 ft (1.5 m) high with a fire-resistance rating of at least 1/2 hour.

Timed Interactive CWI Quiz

Ready for more? Take the full interactive quiz below and see your score at the end.

17

cwi part a practice test

The CWI Part A Practice Test is more than just a simulation of the actual exam - it's a powerful learning tool that can help you identify your strengths, weaknesses, and knowledge gaps. By taking multiple practice tests, you'll become familiar with the exam format, question types, and the breadth of topics covered.

1. A gas flow rate of 30 cfh is what in l/min?

2. Piezoelectricity is a property used by which NDE method?

3. The ability of a metal to absorb energy is called:

4. Which NDT method uses an alternating current coil?

5. A 50.0 lb. can of welding electrodes weighs how many kg?

6. Which of the following tests are referred to as microhardness tests?

7. What weld metal discontinuity results when the welder fails to completely fill the weld groove?

8. MT can be used most effectively to inspect which of the following?

9. The type of alloying in which the alloy atoms are located in the spaces between the atoms of the parent metal is referred to as:

10. Which material property cannot be determined from a tensile test?

11. Test information above the reference line refers to the arrow side.

12. With respect to the rolling direction of steel plate manufacture, which statement is true?

13. The use of preheat will tend to:

14. A discontinuity is:

15. What is the role of the AWS CWI in NDE?

16. The process whereby ultrasonic indications are related to dimensions in a test standard is referred to as:

17. The ‘offset method’ is used for determining which property?

Scored under 80%?Work through every Part A topic with 2,500+ questions, detailed explanations and timed mock exams.

See the question bank →

How to Pass CWI Part A

  • Know the pace. 150 questions in 2 hours is under 50 seconds per question. Answer what you know first, then return to the hard ones.
  • Master welding symbols. Symbol questions are quick marks if you know arrow side versus other side, size versus length and pitch, and the supplementary symbols.
  • Practise the math. Heat input, unit conversions, tensile strength and fillet throat calculations follow a few fixed formulas.
  • Learn causes, not just names. Many questions ask what causes a discontinuity or which NDE method finds it best.
  • Aim for 80%+ in mocks. That gives you a safety margin over the 72% pass mark.

Pass CWI Part A on your first attempt

The complete Part A question bank with realistic mock exams and detailed explanations.

  • 2,500+ questions
  • Mock exams
  • Detailed explanations
  • Free training videos
Start practising →

CWI Part A FAQs

How many questions are on the CWI Part A exam?

Part A (Fundamentals) is a closed-book exam of 150 multiple-choice questions with a 2-hour time limit. You need at least 72% to pass.

What does CWI Part A cover?

Welding processes, metallurgy, welding symbols, terms and definitions, destructive and nondestructive testing, discontinuities, procedures and qualification, inspection calculations and safety.

Is CWI Part A open book?

No. Part A is closed book. Part C (the codebook exam) is the open-book part of the CWI exam.

What is the passing score for each CWI exam part?

You need at least 72% on each of the three parts: Part A (Fundamentals), Part B (Practical) and Part C (Code Book).

How should I use this free CWI practice test?

Take the sample questions without notes, check every explanation, and note the topics you miss. Then practise those topics with timed question sets until you score 80% or more consistently.

Exam format from the American Welding Society. Practice questions are for exam preparation only; always confirm requirements in the current AWS documents and codes.

Leave a Reply